Chrome Core® 8-FM Alloy美国卡朋特Carpenter进口铬铁合金不锈钢化学成分力学物理性能
| Chrome Core® 8-FM Alloy | 
| Type Analysis | ||||||||||||||||||||||||||
| Single figures are nominal except where noted. | ||||||||||||||||||||||||||
| 
 | ||||||||||||||||||||||||||
| General Information | ||
| Description | ||
| Chrome Core® 8 alloy is in a family of controlled chemistry, chromium-iron alloys which are candidates for use in magnetic components where corrosion resistance superior to that of pure iron, low carbon steel and silicon-iron alloys is desired without the substantial decrease in saturation induction associated with the 18% Cr ferritic stainless steels. | ||
| Applications | ||
| Applications could include electro-mechanical devices requiring some degree of corrosion resistance, either in service or for extended shelf life without the need for protective coatings. | ||
| Corrosion Resistance | ||||||
| Chrome Core 8 alloy exhibits no noticeable rusting in 95°F (35°C) - 95% relative humidity tests and have demonstrated corrosion resistance generally similar to 18% chromium ferric stainless steel in certain simulated alcohol-base fuel environments. | ||||||
| Important Note:The following 4-level rating scale is intended for comparative purposes only. Corrosion testing is recommended; factors which affect corrosion resistance include temperature, concentration, pH, impurities, aeration, velocity, crevices, deposits, metallurgical condition, stress, surface finish and dissimilar metal contact. 
 | ||||||
| Properties | ||
| Physical Properties | ||
| Specific Gravity | ||
| -- | 7.70 | |
| Density | ||
| -- | 0.2780 | lb/in³ | 
| Mean Specific Heat | ||
| -- | 0.09930 | Btu/lb/°F | 
| Mean CTE | ||
| 77 to 122°F | 6.20 | x 10-6 in/in/°F | 
| 77 to 212°F | 6.00 | x 10-6 in/in/°F | 
| 77 to 392°F | 6.20 | x 10-6 in/in/°F | 
| 77 to 572°F | 6.40 | x 10-6 in/in/°F | 
| 77 to 752°F | 6.70 | x 10-6 in/in/°F | 
| 77 to 932°F | 6.80 | x 10-6 in/in/°F | 
| 77 to 1112°F | 7.00 | x 10-6 in/in/°F | 
| Modulus of Elasticity (E) | ||
| -- | 29.0 | x 103 ksi | 
| Electrical Resistivity | ||
| 70°F | 295.0 | ohm-cir-mil/ft | 
| Curie Temperature | ||
| -- | 1380 | °F | 
| Magnetic Properties | ||
| Data for fully annealed 0.250-0.625 in. (6.35 to 15.9 mm) diameter bars tested on a Fahy permeameter per ASTM Method A 341. | ||
| Saturation Flux Density | ||
| -- | 18600.0 | G | 
| Coercivity | ||
| -- | 2.50 | Oe | 
| Magnetic Permeability | ||
| -- | 3100.0 | Mu | 
| Residual Induction | ||
| -- | 13800 | G | 
| Typical Mechanical Properties | ||
| Heat Treatment | ||
| Due to the relatively low chromium content, Chrome Core 8 alloy will form austenite if heated to too high a temperature, and some hardening will occur if the austentized part is rapidly cooled. Consequently the best heat treatment for improved soft magnetic properties is to subcritically anneal. | ||
| Workability | ||
| Cold Working | ||
| Chrome Core 8 alloy can be blanked, formed and cold drawn. Cold work will increase the hardness. | ||
| Machinability | ||
| Following are typical feeds and speeds for Chrome Core 8 alloy. | ||
| Additional Machinability Notes | ||
| When using carbide tools, the surface speed can be increased between 2 and 3 times over the high-speed suggestions. Feeds can be increased between 50 and 100%. | ||
| Weldability | ||
| Chrome Core 8 alloy can be satisfactorily welded by shielded fusion and resistance welding processes. Oxyacetylene welding is not recommended. When filler metal is required, consider AWS E/ER430. Post weld heat treatment is desirable for toughness and magnetic performance. Use of austenitic stainless steel filler metal is not recommended due to the magnetic air gap created. | ||
| Other Information | ||||||||
| Forms Manufactured | ||||||||
| 
 | ||||||||
 
 
							 
							 
 
							 
							