通过在Gleeble−l500热模拟试验机上进行等温热压缩试验,研究2E12铝合金在变形温度为300~500 ℃和应变速率为0.0l ~ l0 s−1条件下的流变应力行为,计算、推导出用包含Arrhenius项的Zener-Hollomon参数描述2E12合金高温压缩流变行为的表达式,并分析形变热、变形温度和应变速率等参数对流变应力的影响规律。
2E12铝合金的高温塑性变形流变应力行为Flow stress behavior of 2E12 aluminum alloy during hot plastic deformation at high temperature
通过在Gleeble−l500热模拟试验机上进行等温热压缩试验,研究2E12铝合金在变形温度为300~500 ℃和应变速率为0.0l ~ l0 s−1条件下的流变应力行为,计算、推导出用包含Arrhenius项的Zener-Hollomon参数描述2E12合金高温压缩流变行为的表达式,并分析形变热、变形温度和应变速率等参数对流变应力的影响规律。结果表明:应变速率和变形温度对2E12合金的流变应力影响显著,流变应力随着温度的升高而降低,随着应变速率的提高而增大;在 ≥1 s−1时,形变热导致流变应力降低,且幅度随着应变速率的增大而增大,随着变形温度的升高而降低。
The flow stress behavior of a hot compressed 2E12 aluminum alloy was investigated by compression tests performed on Gleeble−1500 tester at strain rates ranging from 0.01 s−1 to 10 s−1 and temperatures ranging from 300 ℃ to 500 ℃. The expression for describing the rheological behavior of 2E12 alloy during hot compression process by Zener-Hollomon parameter including Arrhenius term was deduced. The influence of temperature rise caused by deformation, testing temperature and strain rate on the flow stress was analyzed. The results show that the flow stress of 2E12 alloy is greatly affected by strain rate and temperature. The flow stress of 2E12 alloy decreases with increasing the temperature and rises with increasing the strain rate. At ≥1 s−1, temperature rise caused by deformation results in reduced flow stress. The decrease of flow stress increases with increasing the strain rate and decreases with increasing the deformation temperature.
作为值得信赖的合作伙伴和高品质金属合金的半成品供应商,艾荔艾拥有完善的服务体系和专业的团队。在同客户交易的过程中,我们力求根据不同的应用需求将我们的产品做到精益求精。针对当前和未来的市场需求,艾荔艾致力于为客户提供最佳的金属材料解决方案。
AILIAI has been a reliable partner and supplier of sophisticated and high-quality semi-finished products maed of alloys. In dialogue with our customers, we optimise our products to meet the specific application requirements. AILIAI develops the best alloy material solutions for current and future challenges.
获取更多我们供应的合金和服务信息,请致电086-021-67660801或发电子邮件kefu@ailiaigroup.com联系我们,您也可以通过微博和微信和我们互动。
For more information on the alloys and services that we supply, call us at 086-021-67660801 or email us at kefu@ailiaigroup.com. You can also get in touch on social media, we are constantly active on Weibo and Weixin.